Polymer Property : Tear Strength = 74.0 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 74.0 kN/m
422 pli
ASTM Die C
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 8 PHR Di-Cup 40C
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
Tear Strength 74.0 kN/m
422 pli
ASTM Die C
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 8 PHR Di-Cup 40C
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
Tear Strength 74.0 kN/m
422 pli
DIN 53515
Lubrizol ESTANE® 5714F1 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..