Mechanical Properties Metric English Comments
Tear Strength 750 kN/m
4280 pli
ASTM D624
GRECO ISOTHANE 3090A Polyether TPU Resin
ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod..
Tear Strength 750 kN/m
4280 pli
ASTM D624
GRECO ISOTHANE 3095A Polyether TPU Resin
ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod..