Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 78.5 kN/m | 448 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® 865A T series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tear Strength | 78.5 kN/m | 448 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® T865A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tear Strength | 78.5 kN/m | 448 pli | Die C; ASTM D624 |
Lubrizol Estane® R175A Thermoplastic Polyurethane Type: Estane® R175A is a Shore 75A, plasticized grade thermoplastic polyurethane (TPU).Uses: Injection Molding.Information Provided by The Lubrizol Corporation |
|||
Tear Strength | 78.5 kN/m | 448 pli | Die C; ASTM D624 |
Lubrizol Estane® R180A Thermoplastic Polyurethane Type: Estane® R180A is a Shore 83A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provi.. |
|||
Tear Strength | 78.5 kN/m | 448 pli | Die C; ASTM D624 |
Lubrizol Estane® S175A Thermoplastic Polyurethane Type: Estane® S175A is a Shore 77A, polyester type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: Americas, Europe, Mid.. |