Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 138 kN/m | 788 pli | |
Axiall EX1264 Moldings & Extrusions Flexible PVC General purpose extrusion compound designed for water stop applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |