Mechanical Properties Metric English Comments
Tear Strength 8.01 kN/m
45.7 pli
212°F, Die C; ASTM D624
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..