Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 8.83 kN/m | 50.4 pli | |
Momentive Performance Materials RTV142 White, Low Volatile, One Component Silicone Sealant RTV 142 one-component, ready-to-use adhesive sealant cures to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. Methyl alcohol vapors are released.. |
|||
Tear Strength | 8.83 kN/m | 50.4 pli | |
Momentive Performance Materials RTV1673LV One Component, Low Volatile Silicone Adhesive Sealant, Black RTV1673LV one-component, ready-to-use adhesive sealants cures to a tough durable, resilient silicone rubber when exposed to atmospheric moisture at room temperature. Methyl alcohol and a small amoun.. |