Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 14.0 kN/m | 80.1 pli | ASTM D624, Die C |
Stellarchem SE/PA745B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |