Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 145 kN/m | 830 pli | ASTM D624 |
Huntsman IROGRAN® A 95 E 4861 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A95 4861 is a high performance polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN A95E 4861 is part of the HUNTSMAN technical extrusion pro.. |
|||
Tear Strength | 145 kN/m | 830 pli | ASTM D624 (Die C) |
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 15N95UV is a polyether copolymer-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis resist.. |