Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 15.0 kN/m @Temperature 21.0 °C |
85.6 pli @Temperature 69.8 °F |
Die C2 hr; ASTM D624 |
PolyOne Versalloy™ XL 9045-1 Thermoplastic Elastomer (TPE) Versalloy™ XL 9045-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | D624 |
Polykemi AB POLYelast TPE Z300 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Tear Strength | >= 15.0 kN/m | >= 85.6 pli | DIN 53507 |
Huntsman AVALON® 55 AEX Thermoplastic Polyurethane Introduction: AVALON 55 AEX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 55 AEX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Tear Strength | 15.0 - 35.0 kN/m | 85.6 - 200 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 5K Polytetrafluoroethylene Coated Kevlar Fabric PTFE coated Kevlar fabric TISOFLON®Information provided by Isoflon. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2730 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Tear Strength | >= 15.0 kN/m | >= 85.6 pli | DIN 53507 |
Karina E 5525/1-TRE Kariprene Natural. Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | >= 15.0 kN/m | >= 85.6 pli | DIN 53507 |
Karina E 6048/1-TRE Kariprene Black Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | Die B |
Momentive Performance Materials HV 3/506 Heat Cured Rubber - High Temperature Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | Die B |
Momentive Performance Materials TSE 221-3U Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | ASTM D624 |
Sumitomo Chemical ESPOLEX® WT446 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | |
Trelleborg B473 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | |
Trelleborg B700 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | |
Trelleborg B800 Commercial Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | |
Trelleborg R448 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | |
Trelleborg R449 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | |
Trelleborg Neoprene® C432 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | ASTM D624 |
ELASTO UK Dryflex® 600350S SEBS Based Material, Filled Qualities, 35A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | ASTM D624 |
ELASTO UK Dryflex® 660400S SEBS Based Material, Semi-Filled Qualities, 40A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tear Strength | 15.0 kN/m | 85.6 pli | ASTM D624 |
ELASTO UK Dryflex® 660450S SEBS Based Material, Semi-Filled Qualities, 45A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |