Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 161 kN/m | 919 pli | ISO 34 |
Chengdu Polyster H7560 Thermoplastic Polyether-ester Elastomer (TPEE) High modulus molding and injection grade. Contains improved color- stable antioxidants. Good balance of modulus and toughness. Parts and components of automobile, wires, cables and optical fiber, ho.. |
|||
Tear Strength | 161 kN/m | 919 pli | ISO 34 |
Chengdu Polyster H7560Y Thermoplastic Polyether-ester Elastomer (TPEE) High modulus molding and extrusion grade. Contains improved color- stable antioxidants. Low frictional coefficient and good abrasion resistance. Spherical socket of ball joint and lock of automobile.. |