Mechanical Properties Metric English Comments
Tear Strength 94.6 kN/m
540 pli
ASTM Die C
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
Tear Strength 94.6 kN/m
540 pli
ASTM Die C
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 400ºF Cure Temperature
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
Tear Strength 94.6 kN/m
540 pli
Die C; ASTM D624
Lubrizol Pellethane® 2363-90AE Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Tear Strength 94.6 kN/m
540 pli
Die C; ASTM D624
Lubrizol Estane® 2103-90AEFH Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product ..
Tear Strength 94.6 kN/m
540 pli
Die C; ASTM D624
Lubrizol Estane® 2103-90AEL Film Grade Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product ..