Mechanical Properties Metric English Comments
Charpy Impact, Unnotched 20.0 J

@Temperature 20.0 °C
14.8 ft-lb

@Temperature 68.0 °F
Transverse
Industeel CLC 1.2312 Prehardened Mold Steel (300HB/32HRC) with Improved Machinability
Description: CLC 1.2312 is a chromium-manganese-molybdenum grade designed for plastic mold industry. This grade is normally delivered in a prehardened condition at a hardness level of 300HB/32HRC. T..