Mechanical Properties Metric English Comments
Flexural Strength 75.57 MPa

@Temperature 121 °C
10960 psi

@Temperature 250 °F
Master Bond EP45HT-1 Adhesive Resists Exposure to Sterilization
Description: Master Bond Polymer System EP45HT-1 is a remarkably fast curing, medium viscosity, two component epoxy compound formulated for high performance casting and bonding. It is 100% reactive ..
Copyright © lookpolymers.com All Rights Reserved