Mechanical Properties Metric English Comments
Flexural Strength 110 MPa

@Temperature 125 °C
16000 psi

@Temperature 257 °F
ISO 178
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, ..
Flexural Strength 110 MPa

@Temperature 232 °C
16000 psi

@Temperature 450 °F
ASTM D790
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with ..
Flexural Strength 110 MPa

@Thickness 1.57 mm
16000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP320E Cotton Fabric
Description: Similar to NP320 with improved moisture resistance. Suitable for electrical applications in moderate humidity conditions.Thickness Tested: 0.062", 0.125", and 0.500”
Flexural Strength 110 MPa

@Thickness 1.57 mm
16000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP347 Cotton Fabric
Description: Bleached canvas with high temperature phenolic resin with molybdenum disulfide lubricant. Low moisture absorption. Capable of 150°C continuous operation.Thickness Tested: 0.062", 0.1..
Flexural Strength 110 MPa

@Thickness 1.57 mm
16000 psi

@Thickness 0.0620 in
LW
Industrial Laminates/Norplex NP631 Paper Base Laminate
Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500"
Flexural Strength 110 MPa

@Thickness 1.57 mm
16000 psi

@Thickness 0.0620 in
LW; ASTM D790
Industrial Laminates/Norplex NP691 Paper Base Laminate
Description: Flame resistant, room temperature punching grade. NP691 is very similar to NP612 in electrical properties and mechanical strength, with improved moisture resistance.Thickness Tested: 0...
Flexural Strength 110 MPa

@Strain 8.00 %
16000 psi

@Strain 8.00 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 15 DUS008 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 15% glass fibers, injection moldingInformation provided by LANXESS.
Flexural Strength 110 MPa

@Temperature 232 °C
16000 psi

@Temperature 450 °F
ASTM D790
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus w..
Flexural Strength 110 MPa

@Temperature -40.0 °C
16000 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-422VOR Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 110 MPa

@Treatment Temp. 200 °C,
Time 3600 sec
16000 psi

@Treatment Temp. 392 °F,
Time 1.00 hour
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t..
Flexural Strength 110 MPa

@Thickness >=150 mm
16000 psi

@Thickness >=5.91 in
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets
Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope..
Flexural Strength 110 MPa

@Strain 5.00 %,
Temperature 23.0 °C
16000 psi

@Strain 5.00 %,
Temperature 73.4 °F
DAM; ASTM D790
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6  (Unverified Data**)
Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers
Flexural Strength 110 MPa

@Temperature 23.0 °C
16000 psi

@Temperature 73.4 °F
ASTM D790
BASF Ultramid® 8202 L Intermediate PA6 (Dry)
Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai..
Flexural Strength 110 MPa

@Treatment Temp. 220 °C,
Time 0.000 sec
16000 psi

@Treatment Temp. 428 °F,
Time 0.000 hour
Four point
BASF Ultramid® Endure D3G7 Glass-Fiber Reinforced Polyamide
Description: Ultramid® Endure is a new, glass-fiber reinforced polyamide that combines excellent heat aging resistance with the good processing properties of PA 66. Ultramid® Endure can withstand ..
Flexural Strength 110 MPa

@Temperature 80.0 °C
16000 psi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-401 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 110 MPa

@Temperature 23.0 °C
16000 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-779 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 110 MPa

@Temperature 125 °C
16000 psi

@Temperature 257 °F
Result based on HT G22; ISO 178
Victrex® HT™ G45 Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia..