Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 115 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 115 MPa

@Temperature 175 °C
16700 psi

@Temperature 347 °F
ISO 178
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, ..
Flexural Strength 115 MPa

@Temperature 175 °C
16700 psi

@Temperature 347 °F
ISO 178
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta..
Flexural Strength 115 MPa

@Strain 6.00 %
16700 psi

@Strain 6.00 %
ISO 178
Lanxess Durethan® B 40 SK 000000 Nylon 6
PA 6, non-reinforced, injection molding
Flexural Strength 115 MPa

@Strain 7.00 %
16700 psi

@Strain 7.00 %
Conditioned; ISO 178
Lanxess Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers
PA 6-Copolymer, 30% glass fibers, injection molding, impact modified, heat-ageing stabilized
Flexural Strength 115 MPa

@Temperature -40.0 °C
16700 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.4%); ASTM-D790
Toyobo GLAMIDE® T-656E Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 115 MPa

@Temperature -40.0 °C
16700 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.8%); ASTM-D790
Toyobo GLAMIDE® T-401 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 115 MPa

@Temperature 175 °C
16700 psi

@Temperature 347 °F
ISO 178
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co..