Flexural Strength 117 MPa

@Thickness 1.57 mm
17000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP310 Cotton Fabric
Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Thickness Tested: 0.062, 0.125", and 0.500".
Flexural Strength 117 MPa

@Thickness 1.57 mm
17000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP313 Cotton Fabric
Description: Canvas phenolic laminate with molybdenum disulfide lubricant. Mechanical properties slightly lower than NP310.Thickness Tested: 0.062", 0.125" & 0.500"
Flexural Strength 117 MPa

@Thickness 1.57 mm
17000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP629 Paper Base Laminate
Description: It is a paper-phenolic high-pressure laminate. It is intended primarily for mechanical applications and is suitable for electrical applications as well. Thickness Tested: 0.062", 0.125"..
Flexural Strength 117 MPa

@Thickness 1.57 mm
17000 psi

@Thickness 0.0620 in
LW; ASTM D790
Industrial Laminates/Norplex NP318 Cotton Fabric
Description: Post-forming canvas phenolic material. Mechanical and electrical properties similar to NP310E. It is made from a cotton fabric weighing more than 4 ounces per square yard and having a t..
Flexural Strength 117 MPa

@Thickness 1.57 mm
17000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP625 Paper Base Laminate
Description: Paper phenolic grade with better moisture resistance than NP612. Requires less heat to punch and shear than NP611.
Flexural Strength 117 MPa

@Temperature 23.0 °C
17000 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-662 Nylon-66