Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 85.8 MPa @Temperature 23.0 °C |
12400 psi @Temperature 73.4 °F |
ASTM D790 |
Daelim H&L Plavis MS Aromatic Polyimide, 15% MoS2 Filled, Machined Parts Available in vacuum or non-lubrication condition, very high abrasion resistance and low friction coefficient propertyInformation provided by Daelim H&L |