Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 125 MPa

@Temperature 23.0 °C
18100 psi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK 450FE20 Polyetheretherketone, 20% PTFE
Product Description:High performance thermoplastic material, 20% filled with PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA foo..
Flexural Strength 125 MPa

@Strain 3.50 %,
Temperature 23.0 °C
18100 psi

@Strain 3.50 %,
Temperature 73.4 °F
ISO 178
Victrex® PEEK 450G General Purpose
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac..
Flexural Strength 125 MPa

@Strain 7.00 %
18100 psi

@Strain 7.00 %
Conditioned; ISO 178
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers
PA 66, 15% glass fibers, injection molding, heat-ageing stabilized
Flexural Strength 125 MPa

@Strain 5.80 %
18100 psi

@Strain 5.80 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant
PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS.
Flexural Strength 125 MPa

@Temperature 80.0 °C
18100 psi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-402FR Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 125 MPa

@Temperature -40.0 °C
18100 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-656E Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 125 MPa

@Temperature -40.0 °C
18100 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 3.5%); ASTM-D790
Toyobo GLAMIDE® T-803 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 125 MPa

@Temperature -40.0 °C
18100 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.4%); ASTM-D790
Toyobo GLAMIDE® NB-1700 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 125 MPa

@Temperature -40.0 °C
18100 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 3.5%); ASTM-D790
Toyobo GLAMIDE® T-802 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 125 MPa

@Temperature 80.0 °C
18100 psi

@Temperature 176 °F
Practical Use (Water Absorption 0.8%); ASTM-D790
Toyobo GLAMIDE® TY-592GHV 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 125 MPa

@Strain 3.50 %,
Temperature 23.0 °C
18100 psi

@Strain 3.50 %,
Temperature 73.4 °F
ISO 178
Victrex® PEEK 381G Medium Viscosity
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD..
Flexural Strength 125 MPa

@Strain 3.50 %,
Temperature 23.0 °C
18100 psi

@Strain 3.50 %,
Temperature 73.4 °F
ISO 178
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac..