Polymer Property : Flexural Strength = 12500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 86.2 MPa

@Temperature 275 °C
12500 psi

@Temperature 527 °F
ISO 178
Victrex® PEEK 450G General Purpose
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac..
Flexural Strength 86.2 MPa

@Temperature 23.0 °C
12500 psi

@Temperature 73.4 °F
ASTM D790
Daelim H&L Plavis N Aromatic Polyimide, Non-Filled, Direct Formed  (Unverified Data**)
Information provided by Daelim H&L
Flexural Strength 86.2 MPa

@Temperature 23.0 °C
12500 psi

@Temperature 73.4 °F
ASTM D790
Daelim H&L Plavis G15 Aromatic Polyimide, 15% Graphite Filled, Direct Formed  (Unverified Data**)
Information provided by Daelim H&L