Polymer Property : Flexural Strength = 1300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 8.96 MPa

@Strain 10.0 %
1300 psi

@Strain 10.0 %
Load Applied Parallel to Fiber Plane, Strain = load deformation in mils for sample 0.5" * 0.5" * 4"
Zircar Ceramics ZAL-45 Alumina Insulation
ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics.
Flexural Strength 8.96 MPa

@Strain 15.0 %
1300 psi

@Strain 15.0 %
Load Applied Normal to Fiber Plane, Strain = load deformation in mils for sample 0.5" * 0.5" * 4"
Zircar Ceramics ZAL-45 Alumina Insulation
ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics.