Polymer Property : Flexural Strength = 13200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 91.0 MPa

@Thickness 1.57 mm
13200 psi

@Thickness 0.0620 in
CW
Industrial Laminates/Norplex NP631 Paper Base Laminate
Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500"
Copyright © lookpolymers.com All Rights Reserved