Mechanical Properties Metric English Comments
Flexural Strength 1520 MPa

@# of Cycles 330000
220000 psi

@# of Cycles 330000
QuesTek® Innovations Ferrium® C64™ Case-hardened Gear Steel with Ultrahigh-strength Core
Description: Ferrium® C64™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the ..
Flexural Strength 1520 MPa

@# of Cycles 550000
220000 psi

@# of Cycles 550000
QuesTek® Innovations Ferrium® C64™ Case-hardened Gear Steel with Ultrahigh-strength Core
Description: Ferrium® C64™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the ..
Flexural Strength 1520 MPa

@# of Cycles 1.20e+6
220000 psi

@# of Cycles 1.20e+6
QuesTek® Innovations Ferrium® C64™ Case-hardened Gear Steel with Ultrahigh-strength Core
Description: Ferrium® C64™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the ..