Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 177 MPa @Strain 5.70 % |
25700 psi @Strain 5.70 % |
cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS. |
|||
Flexural Strength | 177 MPa @Thickness 1.57 mm |
25700 psi @Thickness 0.0620 in |
LW; ASTM D790 |
Industrial Laminates/Norplex NP321 Cotton Fabric
(discontinued **) Description: NP321 consists of a fine weave cotton fabric (linen) impregnated with a phenolic resin binder. Applications include vanes for air and liquid pumps, and compressors. NP321 remains very f.. |