Polymer Property : Flexural Strength = 18000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 124 MPa

@Thickness 1.57 mm
18000 psi

@Thickness 0.0620 in
LW; ASTM D790
Industrial Laminates/Norplex NP310 Cotton Fabric
Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Thickness Tested: 0.062, 0.125", and 0.500".
Flexural Strength 124 MPa

@Thickness 1.57 mm
18000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP310HT Cotton Fabric
Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Designed to meet GE specification A19B15B1Thickness..
Flexural Strength 124 MPa

@Thickness 1.57 mm
18000 psi

@Thickness 0.0620 in
LW; ASTM D790
Industrial Laminates/Norplex NP310HT Cotton Fabric
Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Designed to meet GE specification A19B15B1Thickness..
Flexural Strength 124 MPa

@Thickness 1.57 mm
18000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP319 Cotton Fabric Base Laminate
Description: Bleached canvas combined with phenolic resin and graphite lubricant. Better moisture resistance and machining characteristics than NP315.
Flexural Strength 124 MPa

@Thickness 1.57 mm
18000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP322 Cotton Fabric
Description: Linen phenolic laminate with molybdenum disulfide. Provides the same lubricity as NP313, but has better machining qualities. Mechanical strength similar to, but slightly less than NP320..