Mechanical Properties Metric English Comments
Flexural Strength 182 MPa

@Thickness 1.57 mm
26400 psi

@Thickness 0.0620 in
LW; ASTM D790
Industrial Laminates/Norplex NP680 Paper Base Laminate
Description: Hot punching grade with electrical properties between NP611 to NP631.Thickness Tested: 0.062", 0.125" & 0.500"
Flexural Strength 182 MPa

@Temperature 23.0 °C
26400 psi

@Temperature 73.4 °F
ASTM D790
Saint-Gobain Meldin® 5055 Thermoplastic Bearing Material
General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin..