Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 195 MPa @Strain 4.80 % |
28300 psi @Strain 4.80 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 15 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced PA 6, 15% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Strength | 195 MPa @Temperature -40.0 °C |
28300 psi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-714E Transparent Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |