Polymer Property : Flexural Strength = 215 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 215 MPa

@Temperature 23.0 °C
31200 psi

@Temperature 73.4 °F
ASTM D790
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a low ..
Flexural Strength 215 MPa

@Temperature 23.0 °C
31200 psi

@Temperature 73.4 °F
ASTM D790
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)
Torlon® 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a ..
Flexural Strength 215 MPa

@Temperature 23.0 °C
31200 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 1.75%); ASTM-D790
Toyobo GLAMIDE® T-665C30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..