Polymer Property : Flexural Strength = 220 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 220 MPa

@Temperature 180 °C
31900 psi

@Temperature 356 °F
ISO 178
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica..
Flexural Strength 220 MPa

@Temperature 125 °C
31900 psi

@Temperature 257 °F
ISO 178
Victrex® WG101™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai..
Flexural Strength 220 MPa

@Temperature 125 °C
31900 psi

@Temperature 257 °F
ISO 178
Victrex® WG102™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c..
Flexural Strength 220 MPa

@Treatment Temp. 150 °C,
Time 3600 sec
31900 psi

@Treatment Temp. 302 °F,
Time 1.00 hour
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. UL-94 V..
Flexural Strength 220 MPa

@Temperature 125 °C
31900 psi

@Temperature 257 °F
ISO 178
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co..