Flexural Strength 152 MPa

@Temperature 23.0 °C
22000 psi

@Temperature 73.4 °F
ASTM D790
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only..
Flexural Strength 152 MPa

@Thickness 1.57 mm
22000 psi

@Thickness 0.0620 in
LW; ASTM D790
Industrial Laminates/Norplex NP320E Cotton Fabric
Description: Similar to NP320 with improved moisture resistance. Suitable for electrical applications in moderate humidity conditions.Thickness Tested: 0.062", 0.125", and 0.500”
Flexural Strength 152 MPa

@Thickness 1.57 mm
22000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP600 Paper Base Laminate
Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. This material is most commonly used for drill entry material in the PCB industry. Thickness Tested: 0.062"..
Flexural Strength 152 MPa

@Thickness 1.57 mm
22000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP602 Paper Base Laminate
Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. It is typically hot punched for numerous low voltage, less than 250 volts, electrical applications.Thickne..
Flexural Strength 152 MPa

@Thickness 1.57 mm
22000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP605 Paper Base Laminate
Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. This material is normally used in the printed circuit board industry as a backup for the drilling operatio..
Flexural Strength 152 MPa

@Thickness 1.57 mm
22000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP611 Paper Base Laminate
Description: Hot punching general-purpose phenolic grade. Mechanical properties approach those of NP610 with improved electrical properties and moisture resistance.Thickness Tested: 0.062", 0 125" a..
Flexural Strength 152 MPa

@Thickness 1.57 mm
22000 psi

@Thickness 0.0620 in
LW; ASTM D790
Industrial Laminates/Norplex NP629 Paper Base Laminate
Description: It is a paper-phenolic high-pressure laminate. It is intended primarily for mechanical applications and is suitable for electrical applications as well. Thickness Tested: 0.062", 0.125"..
Flexural Strength 152 MPa

@Thickness 1.57 mm
22000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP660 Paper Base Laminate
Description: Lower cost paper phenolic NEMA Grade XP. Uses natural kraft paper without pigmented cover sheet. Warm to hot punching. UL listed. Thickness Tested: 0.062", 0.125" & 0.500"
Flexural Strength 152 MPa

@Temperature 23.0 °C
22000 psi

@Temperature 73.4 °F
ASTM D790
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
Torlon® 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not ..
Flexural Strength 152 MPa

@Temperature -40.0 °C
22000 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.1%); ASTM-D790
Toyobo GLAMIDE® NB-5620S Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..