Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 240 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 240 MPa

@Temperature 23.0 °C
34800 psi

@Temperature 73.4 °F
DAM; ISO 178
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)
Zytel® 70G25HSL NC010 is a 25% glass fiber reinforced, heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Flexural Strength 240 MPa

@Strain 3.80 %
34800 psi

@Strain 3.80 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® DP BKV 30 XF 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS.
Flexural Strength 240 MPa

@Strain 5.00 %
34800 psi

@Strain 5.00 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® AKV 40 H2.0 901510 Nylon 66, Glass Fiber Reinforced
PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Flexural Strength 240 MPa

@Strain 5.00 %
34800 psi

@Strain 5.00 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® AKV 40 H3.0 000000 Nylon 66, Glass Fiber Reinforced
PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Flexural Strength 240 MPa

@Temperature 23.0 °C
34800 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-669VGB Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 240 MPa

@Thickness >=50.0 mm
34800 psi

@Thickness >=1.97 in
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets
Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope..
Flexural Strength 240 MPa

@Temperature -40.0 °C
34800 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-401 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 240 MPa

@Temperature 23.0 °C
34800 psi

@Temperature 73.4 °F
ASTM D790
DuPont Performance Polymers Rynite® 830ER NC010 PET
Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers
Flexural Strength 240 MPa

@Temperature 23.0 °C
34800 psi

@Temperature 73.4 °F
DAM; ISO 178
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P..