Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 198 MPa @Temperature 23.0 °C |
28700 psi @Temperature 73.4 °F |
ASTM D790 |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |