Mechanical Properties Metric English Comments
Flexural Strength 208 MPa

@Temperature 23.0 °C
30200 psi

@Temperature 73.4 °F
ASTM D790
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with ..
Flexural Strength 208 MPa

@Temperature 23.0 °C
30200 psi

@Temperature 73.4 °F
ASTM D790
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus w..