Mechanical Properties Metric English Comments
Flexural Strength 340 MPa

@Temperature 20.0 °C
49300 psi

@Temperature 68.0 °F
DIN EN 843-1
CeramTec Rocar® SiG Silicon Carbide, SiSiC
Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch..
Flexural Strength 340 MPa

@Temperature 1000 °C
49300 psi

@Temperature 1830 °F
DIN EN 820-1
CeramTec Rocar® SiG Silicon Carbide, SiSiC
Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch..
Flexural Strength >= 340 MPa

@Temperature 23.0 °C
>= 49300 psi

@Temperature 73.4 °F
Perpendicular to laminations; IEC 1212-2 5.1
Hippe EP GC 203 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech..
Flexural Strength >= 340 MPa

@Temperature 23.0 °C
>= 49300 psi

@Temperature 73.4 °F
Perpendicular to laminations; IEC 1212-2 5.1
Hippe EP GC 204 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech..
Flexural Strength >= 340 MPa

@Temperature 23.0 °C
>= 49300 psi

@Temperature 73.4 °F
Perpendicular to laminations; IEC 1212-2 5.1
Hippe EP GC 205 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech..