Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 35.0 MPa

@Temperature 175 °C
5080 psi

@Temperature 347 °F
ISO 178
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, ..
Flexural Strength 35.0 MPa

@Strain 9.00 %
5080 psi

@Strain 9.00 %
Conditioned; ISO 178
Lanxess Durethan® B 40 SK 000000 Nylon 6
PA 6, non-reinforced, injection molding
Flexural Strength 35.0 MPa

@Strain 6.10 %
5080 psi

@Strain 6.10 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® BC 700 HTS DUSXBL 900116 Nylon 6, Impact Modified
PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Flexural Strength 35.0 MPa

@Temperature 23.0 °C
5080 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 2.9%); ASTM-D790
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 35.0 MPa

@Temperature 80.0 °C
5080 psi

@Temperature 176 °F
Practical Use (Water Absorption 1.7%); ASTM-D790
Toyobo GLAMIDE® NB-5550 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 35.0 MPa

@Temperature 23.0 °C
5080 psi

@Temperature 73.4 °F
ASTM D790
BASF Ultramid® 8202 L Intermediate PA6 (Conditioned)
Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai..
Flexural Strength 35.0 MPa

@Strain 6.10 %
5080 psi

@Strain 6.10 %
ISO 178
Lanxess Durethan® BC 700 HTS 900116 Nylon 6/66  (discontinued **)
PA 6/66