Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 270 MPa @Temperature -55.0 °C |
39200 psi @Temperature -67.0 °F |
ISO 178 |
Victrex® PEEK 150GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Flexural Strength | 270 MPa @Strain 3.70 % |
39200 psi @Strain 3.70 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS. |
|||
Flexural Strength | 270 MPa @Temperature -40.0 °C |
39200 psi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-669VGB Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 270 MPa @Temperature 23.0 °C |
39200 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |