Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 417 MPa @Thickness 1.57 mm |
60500 psi @Thickness 0.0620 in |
LW |
Industrial Laminates/Norplex NP185 Carbon Fiber