Mechanical Properties Metric English Comments
Flexural Strength 455 MPa

@Temperature 93.3 °C
66000 psi

@Temperature 200 °F
Dry; ASTM D790
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Flexural Strength 455 MPa

@Temperature 21.1 °C
66000 psi

@Temperature 70.0 °F
Dry; ASTM D790
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Flexural Strength 455 MPa

@Temperature 93.3 °C
66000 psi

@Temperature 200 °F
Dry; ASTM D790
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Flexural Strength 455 MPa

@Thickness 1.57 mm
66000 psi

@Thickness 0.0620 in
CW
Industrial Laminates/Norplex P95 Glass Fabric
Description: Woven glass fabric with polyimide resin engineered to maintain excellent physical properties at 240°C. Low coefficient of thermal expansion, high mechanical strength.Thickness Tested..