Flexural Strength 37.0 MPa

@Temperature 23.0 °C
5370 psi

@Temperature 73.4 °F
ASTM D790
BASF Ultramid® 8270 HS BK 102 PA6 (Conditioned)
Description: Ultramid 8270 HS BK-102 is a thermally modified pigmented black, PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile ex..