Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 55.0 MPa

@Strain 8.00 %
7980 psi

@Strain 8.00 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® DP A 30 S FN30 DUS025 000000 Nylon 66
PA 66, non-reinforced, injection molding, halogen free flame retardant improved flowabilityInformation provided by LANXESS.
Flexural Strength 55.0 MPa

@Strain 7.80 %
7980 psi

@Strain 7.80 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant
PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS.
Flexural Strength 55.0 MPa

@Temperature 80.0 °C
7980 psi

@Temperature 176 °F
Practical Use (Water Absorption 2.3%); ASTM-D790
Toyobo GLAMIDE® T-422-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 55.0 MPa

@Temperature 80.0 °C
7980 psi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-803 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..