Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 593 MPa @Temperature 21.1 °C |
86000 psi @Temperature 70.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Flexural Strength | 593 MPa @Temperature 71.1 °C |
86000 psi @Temperature 160 °F |
Dry; Oven Cure 250°F, 90 min; ASTM D790 |
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra.. |