Flexural Strength 552 MPa

@Temperature 21.1 °C
80000 psi

@Temperature 70.0 °F
Wet; ASTM D790
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Flexural Strength 552 MPa

@Thickness 1.57 mm
80000 psi

@Thickness 0.0620 in
LW; ASTM D790
Industrial Laminates/Norplex NP511 Glass Fabric
Description: Woven glass fabric with high temperature epoxy resin. Excellent mechanical strength and electrical properties at elevated temperatures. Continuous operating temperature is 165°C. Mat..