Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 58.6 MPa

@Temperature 23.9 °C
8500 psi

@Temperature 75.0 °F
Dry; 325°F 2500psi; ASTM D790
Park Electrochemical Nelcote® F-557 Phenolic Prepreg, Chopped Molding Compound Reinforced
Nelcote® F-557 is a high purity silica filler phonic resin coated on Commercial or Aerospace grade silica fabric. F-557 is used in the manufacture of intermediate temperature ablative rocket nozzle..