Polymer Property : Flexural Strength = 87000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 600 MPa

@Temperature 23.9 °C
87000 psi

@Temperature 75.0 °F
Dry; ASTM D790
Park Electrochemical Nelcote® P-670I Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-670I is a versatile, non-styrenated/low VOC polyester resin. P670I is used in a wide variety of applications including radomes, tooling and aircraft structures.Key Features and Benefits:..