Polymer Property : Flexural Strength = 98000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 676 MPa

@Temperature -53.9 °C
98000 psi

@Temperature -65.0 °F
Dry; ASTM D790
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 4581 Quartz
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Flexural Strength 676 MPa

@Thickness 1.57 mm
98000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP545 Carbon Fiber  (discontinued **)
Description: NP545 is composed of carbon fiber fabric and an epoxy resin system. It has excellent moisture resistance and physical properties. Potential uses include fixtures and gage systems, high ..