Shear Strength 0.0829193 - 0.654548 MPa

@Temperature 230 - 250 °C
12.0264 - 94.9343 psi

@Temperature 446 - 482 °F
Average value: 0.314 MPa Grade Count:1
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..
Shear Strength 0.0829193 - 0.654548 MPa

@Shear Rate 50.0 - 5000 1/s
12.0264 - 94.9343 psi

@Shear Rate 50.0 - 5000 1/s
Average value: 0.314 MPa Grade Count:1
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..