Polymer Property : Shear Strength = 0.109 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.109 MPa

@Shear Rate 500 1/s,
Temperature 260 °C
15.8 psi

@Shear Rate 500 1/s,
Temperature 500 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Shear Strength 0.109 MPa

@Shear Rate 500 1/s,
Temperature 260 °C
15.8 psi

@Shear Rate 500 1/s,
Temperature 500 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers