Shear Strength 0.172 MPa

@Temperature 150 °C
25.0 psi

@Temperature 302 °F
Over-Lap Shear on Stainless Steel; ASTM D1002
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Shear Strength 0.172 MPa

@Temperature 150 °C
25.0 psi

@Temperature 302 °F
Over-Lap Shear on Stainless Steel; ASTM D1002
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Shear Strength 0.172 MPa

@Temperature 121 °C
25.0 psi

@Temperature 250 °F
Overlap, Alum/Alum
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive
Features: A light colored, fast drying adhesiveExcellent resistance to aromatic fuels, water and oilUsed to bond many types of plastic films including ABS, cellulose acetate, and PVCInformation prov..