Polymer Property : Shear Strength = 0.965 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.965 MPa

@Temperature 66.0 °C
140 psi

@Temperature 151 °F
1/8" Birch/High-Pressure Laminate, aged 3 mo
3M Fastbond™ 30-NF Contact Adhesive
3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M
Shear Strength 0.965 MPa

@Temperature 66.0 °C
140 psi

@Temperature 151 °F
1/8" Birch/High-Pressure Laminate, aged 3 mo
3M Fastbond™ 30H-NF Contact Adhesive
3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M