Mechanical Properties Metric English Comments
Shear Strength 1.65 MPa

@Time 1.21e+6 sec
240 psi

@Time 336 hour
Graphite Bismaleimide (BMI) composite IM7/5250-4
3M AC-350 Class C-1/2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Shear Strength 1.65 MPa

@Time 1.21e+6 sec
240 psi

@Time 336 hour
Graphite Bismaleimide (BMI) composite IM7/5250-4
3M AC-350 Class C-2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Shear Strength 1.65 MPa

@Time 1.21e+6 sec
240 psi

@Time 336 hour
Graphite Bismaleimide (BMI) composite IM7/5250-4
3M AC-350 Class C-8(24) Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Shear Strength 1.65 MPa

@Temperature -40.0 °C
240 psi

@Temperature -40.0 °F
Overlap, Nylon
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 1.65 MPa

@Temperature -40.0 °C
240 psi

@Temperature -40.0 °F
Overlap, Nylon
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 1.65 MPa

@Temperature -40.0 °C
240 psi

@Temperature -40.0 °F
Overlap, Nylon
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..