Polymer Property : Shear Strength = 10800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 74.5 MPa

@Temperature -53.9 °C
10800 psi

@Temperature -65.0 °F
Short-Beam, Dry; Vacuum/Oven Cured; ASTM D2344
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 3K PW Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Shear Strength 74.5 MPa

@Temperature -55.0 °C
10800 psi

@Temperature -67.0 °F
Fill Short Beam, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber
Information provided by HexCel
Shear Strength 74.5 MPa

@Temperature 104 °C
10800 psi

@Temperature 220 °F
0° Short Beam, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, SGP370-8H Fiber
Information provided by HexCel